Received 17.12.2025
DOI: 10.35556/idr-2026-1(114)62-67
In vitro study of adhesive fixation of metal brackets
Kosyreva T.F.1, ORCID: 0000-0003-4333-5735
Rusanov F.S.2, ORCID: 0000-0001-5280-0294
Orlova O.S.1, ORCID: 0009-0001-7237-3012
Khasan A.M.1, ORCID: 0000-0001-5671-2240
Al-Okbi M.A.1, ORCID: 0000-0001-5216-614X
1 Peoples’ Friendship University of Russia named after Patrice Lumumba
117198, Russia, Moscow, Miklukho-Maklaya St., 6
2 National Medical Research Center for Dentistry and Maxillofacial Surgery of the Ministry of Health of Russia
119021, Russia, Moscow, Timura Frunze St., 16
E-mail address: kosyreva_tf@pfur.ru
Summary
The study investigated the micropermeability of the tooth-adhesive-bracket complex when using metal self-ligating and ligature brackets with «CompoFix Ortho» (Russia) and «Transbond XT» (USA) adhesives. Forty premolars removed for orthodontic reasons and free of caries were used. After the braces were photopolymerized, the teeth were stored in distilled water at room temperature for 1 month, and then subjected to thermal cycling in deionized water at a temperature of 5 ± 2°C to 55 ± 2°C for 500 cycles with a dwell time of 30 seconds and a transfer time of 10 seconds. After thorough washing with distilled water, the samples were air-dried and embedded in acrylic plastic.
It was revealed that the average strength of the adhesive joint when metal braces are detached from tooth enamel, using the composite “CompoFix Ortho” (RF) and the foreign equivalent “Transbond XT” (USA) – 7,6±0,3 MPa, does not statistically differ (p≥0,05), but statistically differs between self-ligated (7,8±0,2 MРa) and ligature braces (7,1±0,15 MРa) (p<0,05).
It was contirmed that the metal braces of different types of ligations cause an increase in the micropermeability of the enamel in the area of the adhesive connection of the fixing material of the bracket with the occlusal and gingival sides of the samples, which can lead to a decrease in the strength of the adhesive connection and the appearance of demineralization: the formation of white spots on the enamel. The study showed no statistical difference between the levels of microleakage of the two compared adhesive systems.
Keywords: self-ligating and ligatured braces, bonding, adhesives, microleakage under braces.
For citation: Kosyreva T.F., Rusanov F.S., Orlova O.S., Khasan A.M., Al-Okbi M.A. In vitro study of adhesive fixation of metal brackets. Stomatology for All / Int. Dental Review. 2026; no. 1 (114): 62–67 (in Russian). doi: 10.35556/idr-2026-1(114)62-67
References
1. Khasan A.M., Kosyreva T.F., Tuturov N.S., Katbeh I., Gharawi A.M., Salman I. Clinical observations of metal brackets detachment using a Russian adhesive com-plex. Stomatology for All / Int. Dental Review. 2023; no. 2 (103): 58–63 (in Russian). doi: 10.35556/idr-2023-2(103)58-63
2. Hedayati Z., Farjood A. Evaluation of Microleakage under Orthodontic Brackets Bonded with Nanocomposites. Contemp Clin Dent. 2018; no. 9 (3): 361–366. doi: 10.4103/ccd.ccd_69_18
3. Shamaa A., Badawy R., El-Sayed W. Microleakage pattern at enamel- adhesive interface under metal brackets bonded with conventional or nano-adhesive systems. Gulf Med J. 2016; no. 5, p. 62–68.
4. Singh S., Brajendu., Haque I., Kavanakudy B.S., Parambil M.H., Soans C.R. Comparative Evaluation of Microleakage below the Orthodontic Brackets after Bonding with Various Adhesive Agents: An In Vitro Study. J Contemp Dent Pract. 2024; no. 25 (8): 722–725. doi: 10.5005/jp-journals-10024-3696
5. Nemer A.S., Razumova S.N., Brago A.S., Artemova O.A. Experimental in vitro study of the adhesive strength of universal adhesives for orthodontic bracket fixation. Russian Journal of Dentistry. 2025; 29, no. 2, p. 143–149 (in Russian). doi: 10.17816/dent646875
6. Razumova SN, Brago AS, Ruda OR, Talandis AG, Khaskhanova LM, Mendosa EYu, Rusanov FS. Adhesive strength of cervical composite restorations. Russian. Journal of Dentistry. 2025; no. 29 (1): 13–20. doi: 10.17816/dent639931
7. Russian Federation Patent for Utility Model “Model for Determining the Strength of the Adhesive Bond of a Bracket with Structural Materials”. Hasan A.M., Kosyreva T.F., Rusanov F.S., Tuturov N.S., Katbekh I. No. 220901 U1 Russian Federation, IPC G09B 23/28, G01N 3/24, A61C 7/12. Applicant Federal State Autonomous Educational Institution of Higher Education “Patrice Lumumba Peoples’ Friendship University of Russia”. Bulletin of the Higher Attestation Commission No. 28, published 10.10.2023, No. RU 220901 U1, Appendix A. (in Russian).
8. Artun J., Bergland S. Clinical trials with crystal growth conditioning as an alternative to acid-etch enamel pretreatment. Am J Orthod. 1984; no. 85 (4): 333-340. doi: 10.1016/0002-9416(84)90190-8
9. Reynolds I.R. A Review of Direct Orthodontic Bonding. British Journal of Orthodontics. 1975; no. 2 (3): 171–178. doi:10.1080/0301228X.1975.11743666